Polymer Property : 200% Modulus = 2.110 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.01455 GPa
2.110 ksi
10 in/min; ASTM D412
PolyOne Elastamax XL-0257-1 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color..