Polymer Property : 200% Modulus = 0.754 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
200% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
200% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
200% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
200% Modulus 0.00520 GPa
0.754 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4640 Low Cost General Purpose Hose
FormulationNordel® IP 4640