Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00328 GPa | 0.475 ksi | ASTM D412 |
Lubrizol Estane® AG 4950 Thermoplastic Polyurethane Type: Estane® AG 4950 is a polyether based aliphatic thermoplastic polyurethane (TPU) specifically formulated to be used as an adhesive interlayer in transparencies for electronic displays, aerospa.. |