Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00315 GPa | 0.457 ksi | 10 in/min; ASTM D412 |
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged.. |