Polymer Property : 200% Modulus = 0.01069 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.01069 GPa
1.550 ksi
10 in/min; ASTM D412
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann..