Mechanical Properties Metric English Comments
200% Modulus 0.00620 GPa
0.899 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00620 GPa
0.899 ksi
ASTM D412
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
200% Modulus 0.00620 GPa
0.899 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00620 GPa
0.899 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 5565 General Purpose Molding
FormulationNordel® IP 5565