Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00579 GPa | 0.840 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
200% Modulus | 0.00579 GPa | 0.840 ksi | |