Polymer Property : 200% Modulus = 0.00480 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00480 GPa
0.696 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00480 GPa
0.696 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00480 GPa
0.696 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00480 GPa
0.696 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..