Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 5700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 39.3 MPa

@Thickness 0.0254 mm
5700 psi

@Thickness 0.00100 in
High Stalk Extrusion - 6:1 FLH/D ratio and 4:1 BUR; ASTM D882A
Total HL 428 HDPE Film Grade
Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro..
Copyright © lookpolymers.com All Rights Reserved