Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dynatup @ -30°C | 81.3 J @Thickness 3.17 mm |
60.0 ft-lb @Thickness 0.125 in |
ARM Std. Low Temp Impact; ARM Std. |
Formosa Plastics Formolene® L63935 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering .. |
|||
Dynatup @ -30°C | 81.3 J @Thickness 3.17 mm |
60.0 ft-lb @Thickness 0.125 in |
ARM Std. Low Temp Impact; ARM Std. |
Formosa Plastics Formolene® L63935U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsFormolene L63935U is fully heat and UV stabilized.Meets all requirements of the U.S. Food and Drug Adminis.. |
|||
Dynatup @ -30°C | 81.3 J @Thickness 3.17 mm |
60.0 ft-lb @Thickness 0.125 in |
ARM Std. Low Temp Impact; ARM Std. |
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the .. |