Mechanical Properties Metric English Comments
Dynatup @ -30°C 38.6 J
28.5 ft-lb
ASTM D3763
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..