Mechanical Properties Metric English Comments
Heat Seal Strength, Ultimate 13.6 N
3.06 lb (f)
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can..