Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hot Tack Strength, Ultimate | 3.80 N | 0.854 lb (f) | |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can.. |