Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Stiffness Modulus | 0.900 GPa | 131 ksi | 3 pt. secant ASTM D790 |
Chevron Phillips HiD® 9308 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 345460A; ASTM D 4976 Classification: PE 235, A 56607Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |