Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dynatup @ -18°C Max Load | 571000 g | 1260 lb | 23°C; D3763 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |