Polymer Property : Izod Impact Resistance = 6.19 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 1.30 J/cm²
6.19 ft-lb/in²
ISO 180
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..