Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 12.3 J/cm² | 58.5 ft-lb/in² | |
Dow HDPE 08454N High Density Polyethylene DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wi.. |