Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 9.50 J/cm² | 45.2 ft-lb/in² | |
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |