Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 180 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |