Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 8.20 J @Thickness 2.70 mm, Temperature -40.0 °C |
6.05 ft-lb @Thickness 0.106 in, Temperature -40.0 °F |
max load; ASTM D3763 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |