Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
d.a.m.; ISO 6603-2 |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |