Mechanical Properties Metric English Comments
Puncture Energy 5.80 J

@Load <=128.7 kg
4.28 ft-lb

@Load <=283.7 lb
cond.; ISO 6603-2
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.