Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |