Polymer Property : Puncture Energy = 5.00 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 5.00 J

@Temperature -30.0 °C
3.69 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.