Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Puncture Energy | 64.0 J @Temperature -30.0 °C |
47.2 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Puncture Energy | 64.0 J @Load <=510 kg, Temperature 23.0 °C |
47.2 ft-lb @Load <=1120 lb, Temperature 73.4 °F |
ISO 6603-2 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Puncture Energy | 64.0 J @Load <=5810 kg, Temperature -30.0 °C |
47.2 ft-lb @Load <=12800 lb, Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |