Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 3.80 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 3.80 J

@Load <=95.3 kg,
Temperature 23.0 °C
2.80 ft-lb

@Load <=210 lb,
Temperature 73.4 °F
ISO 6603-2
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS.
Copyright © lookpolymers.com All Rights Reserved