Polymer Property : Puncture Energy = 16.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 22.0 J

@Temperature -20.0 °C
16.2 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BH345MO Polypropylene Copolymer
BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio..
Puncture Energy 22.0 J

@Temperature -20.0 °C
16.2 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BJ360MO Polypropylene Copolymer
BJ360MO is a heterophasic copolymer. This grade provides unique combination of very high melt flow rate, high impact strength and stiffness. and is designed for high-speed injection molding and cont..