Mechanical Properties Metric English Comments
Secant Modulus 6.74 GPa

@Strain 0.350 %,
Temperature -40.0 °C
978 ksi

@Strain 0.350 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 6.74 GPa

@Strain 0.350 %,
Temperature -40.0 °C
978 ksi

@Strain 0.350 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 6.74 GPa

@Strain 0.360 %,
Temperature 40.0 °C
978 ksi

@Strain 0.360 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..