Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.46 GPa @Strain 1.73 %, Temperature 40.0 °C |
937 ksi @Strain 1.73 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |