Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.35 GPa @Strain 1.04 %, Temperature 23.0 °C |
920 ksi @Strain 1.04 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Secant Modulus | 6.34 GPa @Strain 0.900 %, Temperature -40.0 °C |
920 ksi @Strain 0.900 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |