Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.275 GPa @Strain 1.60 %, Temperature 40.0 °C |
910.1 ksi @Strain 1.60 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |