Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.547 GPa @Strain 6.70 %, Temperature 40.0 °C |
79.4 ksi @Strain 6.70 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Secant Modulus | 0.548 GPa @Strain 12.8 %, Temperature 23.0 °C |
79.4 ksi @Strain 12.8 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |