Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.513 GPa @Strain 7.00 %, Temperature 80.0 °C |
74.4 ksi @Strain 7.00 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |