Mechanical Properties Metric English Comments
Secant Modulus 0.501 GPa

@Strain 6.0764 %,
Temperature 100 °C
72.7 ksi

@Strain 6.0764 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..