Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.90 GPa @Strain 1.85 %, Temperature -20.0 °C |
1150 ksi @Strain 1.85 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Secant Modulus | 7.90 GPa @Strain 0.950 %, Temperature 80.0 °C |
1150 ksi @Strain 0.950 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |