Polymer Property : Secant Modulus = 69.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.476 GPa

@Strain 7.41 %,
Temperature 40.0 °C
69.0 ksi

@Strain 7.41 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal..