Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.44 GPa @Strain 0.250 %, Temperature 40.0 °C |
934 ksi @Strain 0.250 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |