Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.04 GPa @Strain 0.250 %, Temperature 80.0 °C |
876 ksi @Strain 0.250 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Secant Modulus | 6.04 GPa @Strain 1.48 %, Temperature 40.0 °C |
875 ksi @Strain 1.48 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |