Mechanical Properties Metric English Comments
Secant Modulus 5.51 GPa

@Strain 1.40 %,
Temperature -20.0 °C
799 ksi

@Strain 1.40 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.51 GPa

@Strain 1.40 %,
Temperature -20.0 °C
799 ksi

@Strain 1.40 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.51 GPa

@Strain 1.50 %,
Temperature -40.0 °C
799 ksi

@Strain 1.50 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers