Secant Modulus 5.47 GPa

@Strain 2.90 %,
Temperature 0.000 °C
794 ksi

@Strain 2.90 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Secant Modulus 5.47 GPa

@Strain 0.670 %,
Temperature 40.0 °C
793 ksi

@Strain 0.670 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..