Polymer Property : Secant Modulus = 5.45 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.45 GPa

@Strain 0.700 %,
Temperature 23.0 °C
790 ksi

@Strain 0.700 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)  (Unverified Data**)
10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu..