Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.3469 GPa @Strain 1.45 %, Temperature 100 °C |
485.43 ksi @Strain 1.45 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |