Secant Modulus 3.03 GPa

@Strain 1.50 %,
Temperature 80.0 °C
439 ksi

@Strain 1.50 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Secant Modulus 3.03 GPa

@Strain 1.10 %,
Temperature -40.0 °C
439 ksi

@Strain 1.10 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)  (Unverified Data**)
20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe..