Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.7125 GPa @Strain 0.400 %, Temperature -40.0 °C |
683.50 ksi @Strain 0.400 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |