Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.0299 GPa @Strain 41.95 %, Temperature 23.0 °C |
4.34 ksi @Strain 41.95 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT