Polymer Property : Secant Modulus = 35.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.243 GPa

@Strain 0.210 %,
Temperature 40.0 °C
35.2 ksi

@Strain 0.210 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio..