Mechanical Properties Metric English Comments
Secant Modulus 2.375 GPa

@Strain 0.480 %,
Temperature 40.0 °C
344.5 ksi

@Strain 0.480 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..