Mechanical Properties Metric English Comments
Secant Modulus 3.27 GPa

@Strain 1.50 %,
Temperature -40.0 °C
474 ksi

@Strain 1.50 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..
Secant Modulus 3.27 GPa

@Strain 1.60 %,
Temperature -40.0 °C
474 ksi

@Strain 1.60 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..