Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.84 GPa @Strain 1.50 %, Temperature 100 °C |
412 ksi @Strain 1.50 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |