Mechanical Properties Metric English Comments
Secant Modulus 12.4 GPa

@Strain 0.580 %,
Temperature 23.0 °C
1800 ksi

@Strain 0.580 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..